Revealing and reducing growth-induced interfacial disorder in preferentially aligned nitrogen-vacancy centers in diamond
Cheng-I Ho, Marina Davydova, Patrik Straňák, Felix Hoffmann, Peter Knittel, Andrej Denisenko, Jörg Wrachtrup
Fig. 4, panel (e)
Spin-echo decay rate $\Gamma_2$ (kHz) per layer L0 to L3 for sample S1: measured, and projected from the P1-center concentrations and from the SIMS nitrogen concentrations, with error bars.
Files
- Data: data.csv
Provenance
This panel was reproduced from the authors' public data deposit (DaRUS: https://doi.org/10.18419/darus-6396, CC BY 4.0). The plot shown here is re-rendered for interactive viewing and analysis. See the paper for the original figure and full scientific context.
License: CC BY 4.0.
arXiv:2608.02350 · arXiv: 2608.02350
Other panels of Fig. 4: (a-1) (a-2) (b-1) (b-2) (c) (d) (f)